[Problem] To provide a shape memory resin, which has an excellent shape memory effect and shows little color change with the passage of time, and an orthodontic appliance using the shape memory resin. Also provided is a method for controlling the viscoelastic property of a shape memory resin to a desired level.[Solution] An orthodontic appliance is produced by: mixing polyethyl methacrylate with benzoyl peroxide to give powder (A); mixing methyl methacryloyloxyethylsuccinate with 1,6-hexanediol dimethacrylate, adding N,N-dimethyl-p-toluidine thereto, further adding 1-butanol and thoroughly mixing the mixture to give solution (B); mixing powder (A) with solution (B) to give a homogeneous solution; putting the solution into a mold; and polymerizing the same. The viscoelastic property can be controlled by controlling the amount of 1-butanol added in the aforesaid process.
机译:[问题]提供一种形状记忆树脂,其具有优异的形状记忆效果并且随着时间的流逝几乎不显示颜色变化,以及使用该形状记忆树脂的正畸器具。还提供了一种用于将形状记忆树脂的粘弹性控制到期望水平的方法。[解决方案]正畸器具的生产方法是:将聚甲基丙烯酸乙酯与过氧化苯甲酰混合,得到粉末(A);将甲基丙烯酰氧基氧乙基琥珀酸甲酯与1,6-己二醇二甲基丙烯酸酯混合,向其中加入N,N-二甲基-对甲苯胺,进一步加入1-丁醇并充分混合,得到溶液(B)。将粉末(A)与溶液(B)混合,得到均匀溶液;将溶液放入模具中;并聚合相同。粘弹性质可以通过控制在上述方法中添加的1-丁醇的量来控制。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号