PURPOSE: A bio-soluble mineral wool fiber composition and a mineral wool fiber is provided to maintain thermal and physical properties of the mineral wool fiber and to have excellent bio-solubility.;CONSTITUTION: A bio-soluble mineral wool fiber composition comprises 45-67 wt% of sum content of SiO2 and Al2O3, 20.1-50 wt% of sum content of CaO, MgO, Na2O, and K2O, and other components. The bio-soluble mineral wool fiber composition comprises 30-45 wt% of SiO2, 15-22 wt% of Al2O3, 8-12 wt% of iron oxide (including one or more FeO and Fe2O3), 15-30 wt% of CaO, 5-15 wt% of MgO, and 0.1-5 wt% of R2O (including one or more Na2O and K2O). The dissolution rate constant for simulated body fluid of the bio-soluble mineral wool fiber composition is 300ng/cm^2·hr or greater.;COPYRIGHT KIPO 2013
机译:目的:提供一种生物可溶性矿棉纤维组合物和一种矿棉纤维,以维持矿棉纤维的热和物理性能,并具有优异的生物溶解性。;组成:一种生物可溶性矿棉纤维组合物,包含45- SiO 2和Al 2 O 3的合计含量为67重量%,CaO,MgO,Na 2 O和K 2 O及其他成分的合计含量为20.1-50重量%。该生物可溶性矿棉纤维组合物包含30-45重量%的SiO 2,15-22重量%的Al 2 O 3,8-12重量%的氧化铁(包括一种或多种FeO和Fe 2 O 3),15-30重量%的CaO。 ,5-15 wt%的MgO和0.1-5 wt%的R2O(包括一种或多种Na2O和K2O)。生物可溶性矿棉纤维组合物的模拟体液的溶出速度常数为300ng / cm ^ 2·hr以上。COPYRIGHTKIPO 2013

著录项

  • 公开/公告号KR20120116235A

    专利类型

  • 公开/公告日2012-10-22

    原文格式PDF

  • 申请/专利权人 KCC CORPORATION;

    申请/专利号KR20110033853

  • 申请日2011-04-12

  • 分类号C03C13/06;C03C3/062;D01F9/08;C03B37/00;

  • 国家 KR

  • 入库时间 2022-08-21 17:08:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号