首页> 外国专利> Method for producing a dust collecting filter using a loofah , a natural material

Method for producing a dust collecting filter using a loofah , a natural material

机译:使用天然材料丝瓜络制造集尘过滤器的方法

摘要

PROBLEM TO BE SOLVED: To develop and provide a method of manufacturing a dust collection filter using loofah fibers having good dust collection efficiency by applying various kinds of processing to dried loofah made of only fibers obtained from loofah after ripening as a cucurbit.;SOLUTION: The method of manufacturing the dust collection filter includes: a step of forming a dried loofah (1) having a proper diameter (X) and a length (Y) into a cylindrical shape by removing a core of a central part supported by fibers; a step of immersing the dried loofah (1) formed into the cylindrical shape into warm water having a proper temperature, so that the water sufficiently spreads over a network structure having porosity with various shapes and a fine framework structure and the fibers are swollen; a step of taking up the loofah swollen by the immersion into the warm water from the warm water and holding it between two take-up plates (A, A) and pressing it with a proper pressure; a step of drying the held loofah as it is in a constant-temperature chamber having an inner temperature kept in a range of 60 to 70°C for about four hours; and a step of compressing the dried loofah originally having the cylindrical shape into a plate shape.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:通过对仅由成熟后的丝瓜获得的纤维制成葫芦丝的干燥丝瓜进行各种处理,以开发和提供一种使用具有良好集尘效率的丝瓜纤维制造集尘过滤器的方法;解决方案:该集尘过滤器的制造方法包括以下步骤:通过去除由纤维支撑的中央部分的芯,将具有适当直径(X)和长度(Y)的干燥的丝瓜络(1)制成圆柱形。将干燥后的圆筒状丝瓜络(1)浸入适当温度的温水中,使水充分散布在具有各种形状的孔隙率且骨架结构良好的网状结构上,使纤维溶胀。将丝瓜从热水中浸入温水中以使其膨胀的步骤,然后将其固定在两个卷纸盘(A,A)之间,并用适当的压力对其进行按压;在内部温度保持在60至70℃的恒温室内将保持的丝瓜原样干燥约4小时的步骤; ;以及将原本具有圆筒形的干燥丝瓜络压缩成板状的步骤。;版权所有:(C)2012,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号