Disclosed is a process for the preparation of electroconductive polymer composite based on poly-3,4-ethylenedioxythiophene-polystyrene sulfonate (PEDOT-PSS). Mixed are 8-99 wt. % of PEDOT-PSS and 92-1 wt.% of polyethyleneoxide (PEO), dimethyl sulfoxide or dimethylformamide, or ethylene glycol as organic solvent in concentration of 6-24 vol.% is added to aqueous mixture of PEDOT-PSS and PEO from which composite films are formed. Composite polymeric material prepared is annealed at a temperature of 60- for 10-20 hours.
机译:公开了一种基于聚-3,4-乙撑二氧噻吩-聚苯乙烯磺酸盐(PEDOT-PSS)的导电聚合物复合材料的制备方法。混合的是8-99 wt。将浓度为6-24%(体积)的PEDOT-PSS和92-1 wt。%的聚环氧乙烷(PEO),二甲基亚砜或二甲基甲酰胺或乙二醇作为有机溶剂,添加到形成了哪些复合膜。将制得的复合聚合物材料在60-℃的温度下退火10-20小时。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号