首页> 外国专利> Introducing defined line of weakness by removal of material to fibrous covering material, comprises directing pulsed laser beam to rear side of material and linearly guiding, and determining depth of score line of impingement of laser beam

Introducing defined line of weakness by removal of material to fibrous covering material, comprises directing pulsed laser beam to rear side of material and linearly guiding, and determining depth of score line of impingement of laser beam

机译:通过将材料去除到纤维覆盖材料中来引入定义的薄弱线,包括将脉冲激光束引导到材料的背面并进行线性引导,以及确定激光束的刻痕线深度

摘要

Introducing a defined line of weakness (2) by removal of material to a fibrous covering material (1), comprises directing a pulsed laser beam (31) to the rear side of covering material having display side (11) and a rear side (12) opposite to it, and linearly guiding; and determining a depth of the resulting score line of impingement of a laser beam along a line in each case by many laser pulses. The linear guiding is a multiple repetition of a scanning, and only one laser pulse is emitted, respectively per point of incidence when guided along the line. Introducing a defined line of weakness (2) by removal of material to a fibrous covering material (1), comprises directing a pulsed laser beam (31) to the rear side of covering material having display side (11) and a rear side (12) opposite to it, and linearly guiding; and determining a depth of the resulting score line of impingement of a laser beam along a line in each case by many laser pulses. The linear guiding is a multiple repetition of a scanning, and only one laser pulse is emitted, respectively per point of incidence when guided along the line, which causes an energy input leading to the respective point of incidence to the heating of the fibrous coating material to a temperature above an ablation threshold and maintains a temperature adjacent to the areas of point of incidence of the fibrous coating material below a limit temperature that would lead to changes in the structure of the fibrous coating material.
机译:通过将材料去除到纤维覆盖材料(1)上来引入限定的弱化线(2),包括将脉冲激光束(31)引导到具有显示面(11)和背面(12)的覆盖材料的背面)与之相对,并线性导向;确定在每种情况下通过许多激光脉冲沿激光束撞击的所得刻痕线的深度。线性引导是扫描的多次重复,当沿着直线引导时,每个入射点分别仅发射一个激光脉冲。通过将材料去除到纤维覆盖材料(1)上来引入限定的弱化线(2),包括将脉冲激光束(31)引导到具有显示面(11)和背面(12)的覆盖材料的背面)与之相对,并线性导向;确定在每种情况下通过许多激光脉冲沿激光束撞击的所得刻痕线的深度。线性引导是扫描的多次重复,当沿着直线引导时,每个入射点分别只发射一个激光脉冲,这会导致能量输入,从而导致相应的入射点加热纤维涂层材料加热至高于烧蚀阈值的温度,并将与纤维涂层材料的入射点区域相邻的温度保持在极限温度以下,该极限温度会导致纤维涂层材料的结构发生变化。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号