首页> 外国专利> TRANSITION METAL HEXACYANOFERRATE BATTERY CATHODE, TRANSITION METAL HEXACYANOFERRATE CATHODE BATTERY, METHOD FOR SYNTHESIZING A TRANSITION METAL HEXACYANOFERRATE BATTERY MATERIAL, METHOD FOR FABRICATING A TRANSITION METAL HEXACYANOFERRATE BATTERY CATHODE ELECTRODE, AND METHOD FOR USING A TRANSITION METAL HEXACYANOFERRATE BATTERY

TRANSITION METAL HEXACYANOFERRATE BATTERY CATHODE, TRANSITION METAL HEXACYANOFERRATE CATHODE BATTERY, METHOD FOR SYNTHESIZING A TRANSITION METAL HEXACYANOFERRATE BATTERY MATERIAL, METHOD FOR FABRICATING A TRANSITION METAL HEXACYANOFERRATE BATTERY CATHODE ELECTRODE, AND METHOD FOR USING A TRANSITION METAL HEXACYANOFERRATE BATTERY

机译:过渡金属六氰基高铁电池正极,过渡金属六氰基铁酸铝电池的合成方法,过渡金属六氰基铁酸铝电池材料的制备方法,过渡金属六氰基铁酸锂电池电极的过渡金属制备方法以及方法

摘要

A transition metal hexacyanoferrate (TMH) cathode battery is provided. The battery has a AxMn[Fe(CN)6]y .zH2O cathode, where the A cations are either alkali or alkaline-earth cations, such as sodium or potassium, where x is in the range of 1 to 2, where y is in the range of 0.5 to 1, and where z is in the range of 0 to 3.5. The AxMn[Fe(CN)6]y .zH2O has a rhombohedral crystal structure with Mn2+/3+ and Fe2+/3+ having the same reduction/oxidation potential. The battery also has an electrolyte, and anode made of an A metal, an A composite, or a material that can host A atoms. The battery has a single plateau charging curve, where a single plateau charging curve is defined as a constant charging voltage slope between 15% and 85% battery charge capacity. Fabrication methods are also provided.
机译:提供了过渡金属六氰合铁酸盐(TMH)阴极电池。电池具有AxMn [Fe(CN)6] y .zH2O阴极,其中A阳离子为碱金属或碱土金属阳离子,例如钠或钾,其中x的范围为1至2,其中y为在0.5到1的范围内,其中z在0到3.5的范围内。 AxMn [Fe(CN)6] y .zH2O具有菱形的晶体结构,其中Mn2 + / 3 +和Fe2 + / 3 +具有相同的还原/氧化电位。电池还具有电解质,阳极由A金属,A复合材料或可容纳A原子的材料制成。电池具有单一平稳充电曲线,其中单一平稳充电曲线定义为介于15%和85%电池充电容量之间的恒定充电电压斜率。还提供了制造方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号