首页> 外国专利> NARROW GROOVE TANDEM SUBMERGED ARC WELDING METHOD

NARROW GROOVE TANDEM SUBMERGED ARC WELDING METHOD

机译:窄槽串联埋弧焊方法

摘要

PROBLEM TO BE SOLVED: To provide, in a narrow groove tandem submerged arc welding method of improved 9Cr-1Mo steel, a welding method which is excellent in welding efficiency, satisfactory in a slag peeling efficiency and a bead state, and which can suppress the occurrence of a hot crack of molten metal.SOLUTION: A narrow groove tandem submerged arc welding method uses as a mother material an improved 9Cr-1Mo steel containing C, Si, Mn, P, S, Ni, Cr, Mo, V, Nb, Al, Ti, Zr and N in predetermined quantities, and the remainder being Fe and an inevitable impurity, and a welding wire containing C, Si, Mn, P, S, Ni, Cr, Mo, V, Nb, N and O at predetermined quantities, and the remainder being Fe and an inevitable impurity and having a wire diameter of 4.0 mm, uses an AC power source indicating depending characteristics with the combination of said welding wire and a welding flux of a predetermined alkaline degree, and performs the welding under the predetermined conditions of a wire feeding speed Vof the preceding electrode, a wire feeding speed Vof the trailing electrode, a welding speed v, and the deposition quantity per unit length.SELECTED DRAWING: None
机译:解决的问题:在改进的9Cr-1Mo钢的窄槽串联埋弧焊方法中,提供一种焊接效率优异,熔渣剥离效率和焊道状态令人满意,并且能够抑制焊缝变形的焊接方法。解决方案:窄槽串联埋弧焊方法使用一种改进的9Cr-1Mo钢作为母材,该钢包括C,Si,Mn,P,S,Ni,Cr,Mo,V,Nb ,Al,Ti,Zr和N为预定量,其余为Fe和不可避免的杂质,以及含有C,Si,Mn,P,S,Ni,Cr,Mo,V,Nb,N和O的焊丝焊丝直径为4.0毫米,其余为铁和不可避免的杂质,剩余量为铁和不可避免的杂质,使用交流电源指示所述焊丝和预定碱度的焊剂的结合特性,并执行在送丝规格的预定条件下进行焊接前电极的ed V,尾电极的送丝速度V,焊接速度v和每单位长度的沉积量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号