The present invention relates to a biomaterial having enhanced rubber properties through natural cross-linkage of collagen and hyaluronic acid, a preparing method thereof, and a using method thereof. To this end, the present invention is characterized in that a rubber type biomaterial is prepared by natural cross-linkage of collagen and hyaluronic acid at a ratio of 2:1 to 7:1. The present invention as described above creates a novel material exhibiting rubber properties by providing the conditions for natural cross-linkage rather than chemical or physical cross-linkage and mixing at the optimum ratio of collagen and hyaluronic acid considering their molecular structural features, thereby significantly improving quality and reliability of products, thus meeting a variety of user or customer needs to present a good image.
机译:本发明涉及通过胶原和透明质酸的天然交联而具有增强的橡胶性能的生物材料,其制备方法及其使用方法。为此,本发明的特征在于,通过胶原和透明质酸以2∶1至7∶1的比例自然交联来制备橡胶类生物材料。如上所述的本发明通过提供天然交联而不是化学或物理交联的条件,并考虑到它们的分子结构特征,以胶原蛋白和透明质酸的最佳比例混合来产生具有橡胶特性的新型材料。产品的质量和可靠性,从而满足各种用户或客户的需求,呈现出良好的形象。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号