[PROBLEMS] To provide an organic EL rod-free lead-free glass material which does not contain a metal powder and which can obtain a good sealing quality by laser sealing, has excellent low temperature softening property and stability at the time of melting and has a small thermal expansion coefficient, And high sealing performance and high sealing strength can be achieved at a high yield without requiring strict control of sealing conditions. [MEANS FOR SOLVING PROBLEMS] In order to achieve the above object, according to the present invention, there is provided a method of manufacturing a semiconductor device, comprising: 30 to 60% of V 2 O 5 , 5 to 20% of ZnO, 5 to 20% of BaO, 15 to 40% of TeO 2 , 0 to 7% of Nb 2 O 5 , 0 to 7% of Al 2 O 3 , 0 to 5% of SiO 2 , 0 to 5% of MgO, 0 to 5% of Sb 2 O 3 , 0 to 4% of CuO and 0 to 4% of SnO And an organic EL rod having a glass composition in which Nb 2 O 5 + Al 2 O 3 is 0.5 to 10%, SiO 2 + MgO + Sb 2 O 3 is 0 to 5%, and CuO + SnO is 0 to 4% Lead - free glass.
机译:[问题]提供一种不包含金属粉并且可以通过激光密封获得良好的密封质量,具有优异的低温软化性和熔融时的稳定性并且具有以下特性的有机EL无棒无铅玻璃材料。热膨胀系数小,并且不需要严格控制密封条件就可以以高产率获得高密封性能和高密封强度。 [用于解决问题的手段]为了实现上述目的,根据本发明,提供了一种半导体器件的制造方法,其包括:30%至60%的V 2 O 5 ,ZnO的5%至20%,BaO的5%至20%,TeO 2 的15%至40%,Nb 2 的0%至7% O 5 ,Al 2 的0至7%O 3 ,SiO 2 的0至5%,0 MgO的5%,Sb 2 O 3 的5%,CuO的0%至4%和SnO的0%至4% Nb 2 O 5 + Al 2 O 3 的玻璃组成为0.5%至10%,SiO 2 + MgO + Sb 2 O 3 为0至5%,CuO + SnO为0至4%的无铅玻璃。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号