The present invention relates to a process for the preparation of an organic surfactant comprising the steps of: a) providing an aqueous solution of an organic surfactant; b) providing an aqueous solution of an iron (II) salt and mixing an aqueous solution of the iron (II) salt with an aqueous solution of phosphate to form an iron (II) salt / salt having a stoichiometric ratio of Fe 2+ : Providing a phosphate mixture solution; c) adding said iron (II) salt / phosphate mixed solution to said surfactant solution with continuous stirring; d) providing an aqueous solution comprising a lithium salt, and adding an aqueous solution comprising the lithium salt to the iron (II) salt / phosphate mixed solution to form an aqueous solution comprising about 1: 1: 3 Fe 2+ : Providing a mixture having a stoichiometric ratio, and stirring the resulting mixture; e) heating the resultant mixture at 80-200 占 폚; f) washing the precipitate obtained to remove excess surfactant, filtering and drying the precipitate; And g) provide a method for producing LiFePO 4 powder comprising the step of heat-treating the dried precipitate is fired at 550-850 ℃ for at least 2 hours in an inert atmosphere, the co-solvent in this step (a) to (d) , Or after any one of the steps.
机译:本发明涉及一种制备有机表面活性剂的方法,该方法包括以下步骤:a)提供有机表面活性剂的水溶液; b)提供铁(II)盐的水溶液并将铁(II)盐的水溶液与磷酸盐水溶液混合以形成铁(II)盐/化学计量比为Fe的盐 2 + :提供磷酸盐混合溶液; c)在连续搅拌下将所述铁(II)盐/磷酸盐混合溶液加入到所述表面活性剂溶液中; d)提供包含锂盐的水溶液,并将包含锂盐的水溶液添加到铁(II)盐/磷酸盐混合溶液中以形成包含约1 :: 1:3 Fe 2+ < /:提供具有化学计量比的混合物,并搅拌所得混合物; e)在80-200占폚下加热所得混合物; f)洗涤得到的沉淀以除去过量的表面活性剂,过滤并干燥沉淀; g)提供一种制备LiFePO 4 粉末的方法,该方法包括将干燥的沉淀物在惰性气氛中于550-850℃下煅烧至少2小时的步骤,所述共溶剂为步骤(a)到(d),或在任一步骤之后。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号