POLYOLEFIN-BASED RESIN PRE-EXPANDED PARTICLE, IN-MOLD FOAMED ARTICLE, PROCESS FOR PRODUCING THE POLYOLEFIN-BASED RESIN PRE-EXPANDED PARTICLE, AND PROCESS FOR PRODUCING THE IN-MOLD FOAMED ARTICLE

机译:聚烯烃基树脂预膨胀颗粒,模内发泡制品,生产方法,聚烯烃模制泡沫制品,模内发泡制品的生产过程

摘要

A polyolefin-based resin pre-expanded particle includes a polyolefin-based resin; an organic phosphorus-containing compound being nitrogen-free; and a hindered amine having an OR group substituted directly on an N-atom where R is a saturated or unsaturated hydrocarbyl group, wherein the organic phosphorus-containing compound is at least one selected from the group consisting of alkyl phosphonic acid, an ester of the alkyl phosphonic acid, aryl phosphonic acid, an ester of the aryl phosphonic acid, a cyclic phosphonate, and a cyclic bisphosphonate, the polyolefin-based resin pre-expanded particle comprises from 1.0% by weight to 10% by weight of the organic phosphorus-containing compound and from 0.1% by weight to 5.0% by weight of the hindered amine, and the weight ratio of the organic phosphorus-containing compound to the hindered amine is from 1.0 to 20.
机译:聚烯烃基树脂预发泡颗粒包括聚烯烃基树脂;和一种不含氮的有机含磷化合物;以及R为饱和或不饱和烃基的,在N原子上直接取代有OR基团的受阻胺,其中,有机含磷化合物为选自烷基膦酸(其酯类)中的至少一种。烷基膦酸,芳基膦酸,芳基膦酸的酯,环状膦酸酯和环状双膦酸酯,聚烯烃类树脂预发泡颗粒占有机磷的重量百分比为1.0%至10%。含有0.1重量%至5.0重量%的受阻胺,且有机含磷化合物与受阻胺的重量比为1.0至20。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号