process of obtaining chemical composition for active addition production capable of substituting portland clinker, chemical composition and use of this composition. process for obtaining a chemical composition for the production of active addition capable of substituting portland clinker comprising the following steps: (a) chemical treatment: to the residue the processing of bauxite is added limestone or calcium carbonate derivatives and sand or silica derivatives or silica clays to a sodium content of 30%, of ca 10% and not 10%; preferably sodium 2 between 30 to 40%, ca. 10 to 150%, and not between 4 and 6.0%; (b) homogenization step: the mixture obtained in the previous item undergoes the homogenization process; (c) heat treatment: thereafter the mass of the mixture obtained in process (b) is heated to a temperature between 100000 to 15000c with partial melting and color change; (d) cooling: the cooling process occurs in a satellite or grid chiller; (e) final product: the final product is that obtained when the color of the active addition is dark gray, with performance similar to fly ash and the presence of free dog less than 1.0%; (f) milling: the final product is then subjected to the milling process in conjunction with portland cement clinker to produce cements containing the active addition according to Brazilian standard nbr 12653.
机译:获得能够代替硅酸盐熟料的活性加成产品的化学组成的方法,化学组成和该组成的用途。获得用于生产能够代替硅酸盐熟料的活性添加剂的化学组合物的方法,该方法包括以下步骤:(a)化学处理:将铝土矿的残渣中加入石灰石或碳酸钙衍生物以及沙子或二氧化硅衍生物或二氧化硅粘土来处理铝土矿钠含量> 30%,约> 10%,而不是<10%;最好是钠2在30%至40%之间。 10%至150%,且不在4%至6.0%之间; (b)均质化步骤:将上一项中获得的混合物进行均质化处理; (c)热处理:此后,将在步骤(b)中获得的混合物的质量加热至100000至15000c之间的温度,部分熔融并改变颜色; (d)冷却:冷却过程发生在卫星或电网冷却器中; (e)最终产品:最终产品是当活性添加物的颜色为深灰色,性能与粉煤灰相似且游离狗的含量小于1.0%时获得的产品; (f)研磨:然后将最终产品与硅酸盐水泥熟料一起进行研磨工艺,以生产根据巴西标准nbr 12653所含活性添加剂的水泥。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号