Provided are a sulphur-carbon composite for a lithium-sulphur battery and a preparation method therefor, and an electrode material and a lithium-sulphur battery containing the sulphur-carbon composite. The composite comprises carbon nanoparticles, sulphur loaded in the carbon nanoparticles and a silicon dioxide template agent remaining in the carbon nanoparticles, wherein, by mass percent, the sulphur content is 40%-70% and the content of the silicon dioxide template agent is 0.3%-3%. The residual silicon dioxide template agent is dispersed in the carbon nanoparticles so as to reduce the pore diameter of the carbon nanoparticles.
机译:提供一种用于锂硫电池的硫碳复合物及其制备方法,以及包含该硫碳复合物的电极材料和锂硫电池。该复合材料包括碳纳米颗粒,负载在碳纳米颗粒中的硫和残留在碳纳米颗粒中的二氧化硅模板剂,其中,按质量百分比计,硫含量为40%-70%,二氧化硅模板剂的含量为0.3 %-3%。残留的二氧化硅模板剂分散在碳纳米颗粒中,以减小碳纳米颗粒的孔径。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号