the object of the application is a way of manufacturing products flexible plywood, intended especially for manufacturing shaped in two planes such as the backrest and the seat chairs and chairs and other items used in the production of furniture with the elements giu0119tymi.the way is that in the first stage is initially composed of natural external panel veneer thickness 0.45 - 0,8 mm, flizeliny weighing 85 - 180 g / m2 coated adhesive termotopliwym, preferably acrylic and a single layer u0142uszczki bukowej thickness 0.85 - 12 mm, coated urea formaldehydowym unilaterally adhesive and panel are pressing in the form of temperature 80 - 95u00b0c during 60 - 90 s, and then, in the second stage formatku0119 composed of u0142uszczki bukowej about 4 - 8% moisture content and thickness of 0.8 - 1.3 mm with imposed unilaterally in quantities of 110 to 160 g / m2, adhesive, urea formaldehydowym,the final element of ensuring the thickness after pressing in the 3 - 30 mm, with the outside panels uformowanymi initially in the first stage to a temperature of not less than 100 degrees, they are under pressure not lower than 10 kg / cm2 in the form at a temperature of approximately 60 - 120u00b0c by period of 270 - 480 p.
机译:本申请的目的是一种制造柔性胶合板的方法,该胶合板特别用于制造在两个平面中成形的形状,例如靠背,座椅和椅子以及用于家具生产的具有gi u0119tymi元素的其他物品。是在第一步中,最初是由天然外面板贴面厚度0.45-0.8毫米,重量为85-180 g / m2的涂胶粘合剂,最好是丙烯酸和单层厚度0.85-12毫米的flizeliny组成,在60-90 s内以80-95 u00b0c的形式对涂覆的脲醛缩醛单面胶和面板进行加压,然后在第二阶段由大约4-8%的水分含量和厚度的胶布压制。 0.8-1.3 mm,单面施涂量为110至160 g / m2,粘合剂,尿素甲醛,确保压入3-30 mm后厚度的最终要素面板uformowanymi最初在第一阶段达到不低于100度的温度,并且处于不低于10 kg / cm2的压力下,处于大约60-120 u00b0c的温度下,持续时间为270-480 p 。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号