摘要

the composition of the invention is based on oxides of zirconium, cerium and at least one other of the rare earth cu00e9hum with cerium oxide content of not more than 50% by mass, and it is after calcination at 1000 c, 6 hours, the maximum temperature of the ru00e9ductibilitu00e9 in a specific surface area of at least 45 m2 / g.it is prepared by a process in which we reacted continuously a mixture of compounds of zirconium, cerium and other rare earth compound with a base with a residence time of at most 100 milliseconds, and the precipitate is heated and brought into contact with a surfactant at after being calcined.
机译:本发明的组合物基于锆,铈和至少一种稀土铈的氧化物,氧化铈含量不超过50质量%,并且是在1000℃下煅烧6小时后,比表面积的最高温度至少为45 m2 / g。它是通过使锆,铈和其他稀土化合物与碱的停留时间至多为100毫秒,并且将沉淀物加热并在煅烧后使其与表面活性剂接触。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号