The present invention provides a novel Fe-Mn-Si-based alloy casting material which is useful as a construction material and the like and has excellent low-cycle fatigue properties. According to one embodiment of the present invention, the Fe-Mn-Si-based alloy casting material is characterized by containing Mn and Si as essential component elements and containing at least one among Cr, Ni, Al, and C as optional component elements, the composition of the alloy casting material being 5 mass% ≤ Mn ≤ 35 mass%, 1.5 mass% ≤ Si ≤ 6.5 mass%, 0 mass% ≤ Cr ≤ 15 mass%, 0 mass% ≤ Ni≤ 15 mass%, 0 mass% ≤ Al ≤ 3 mass%, and 0 mass% ≤ C ≤ 0.4 mass%, with the remainder comprising Fe and unavoidable impurities, wherein the conditions of formula (A), 37[%Mn]+0.3[%Si]+0.7[%Cr]+2.4[%Ni]+5.2[%Al]+28[%C]45, and formula (B), [%Ni]+30[%C]+0.5[%Mn]0.75[%Cr]+1.125[%Si]+2[%Al] are satisfied.
机译:本发明提供了新型的Fe-Mn-Si基合金铸造材料,其可用作建筑材料等并且具有优异的低周疲劳性能。根据本发明的一个实施方式,Fe-Mn-Si基合金铸造材料的特征在于,含有Mn和Si作为必要的组成元素,并且含有Cr,Ni,Al和C中的至少一种作为可选的组成元素,合金铸造材料的组成为5质量%≤Mn≤35质量%,1.5质量%≤Si≤6.5质量%,0质量%≤Cr≤15质量%,0质量%≤Ni≤15质量%,0质量%≤Al≤3质量%,0质量%≤C≤0.4质量%,其余部分包含Fe和不可避免的杂质,其中式(A)的条件为37 <[%Mn] +0.3 [%Si] + 0.7 [%Cr] +2.4 [%Ni] +5.2 [%Al] +28 [%C] <45,且式(B),[%Ni] +30 [%C] +0.5 [%Mn]> 0.75满足[%Cr] +1.125 [%Si] +2 [%Al]。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号