The present invention provides a new Fe-Mn-Si-based cast alloy having excellent low-cycle fatigue properties that is useful as a structural building material or the like. An Fe-Mn-Si-based cast alloy according to one embodiment of the present invention contains Mn and Si as an essential component element, and one or more of Cr, Ni, Al, and C as an optional component element. The Fe-Mn-Si-based cast alloy has a component composition being 5 mass% ≤ Mn ≤ 35 mass%, 1.5 mass% ≤ Si ≤ 6.5 mass%, 0 mass% ≤ Cr ≤ 15 mass%, 0 mass% ≤ Ni ≤ 15 mass%, 0 mass% ≤ Al ≤ 3 mass%, and 0 mass% ≤ C ≤ 0.4 mass%, with the balance being Fe and inevitable impurities, and the component composition satisfies conditions of Formula (a): 37 [%Mn] + 0.3[%Si] + 0.7[%Cr] + 2.4[%Ni] + 5.2[%A] + 28[%C] 45, and Formula (b): [%Ni] + 30[%C] + 0.5[%Mn] 0.75[%Cr] + 1.125[%Si] + 2[%Al].
机译:本发明提供了具有优异的低循环疲劳特性的新型Fe-Mn-Si基铸造合金,其可用作建筑建材等。根据本发明的一个实施方式的Fe-Mn-Si基铸造合金包含Mn和Si作为必要的构成元素,以及Cr,Ni,Al和C中的一种或多种作为任选的构成元素。 Fe-Mn-Si系铸造合金的成分组成为5质量%≤Mn≤35质量%,1.5质量%≤Si≤6.5质量%,0质量%≤Cr≤15质量%,0质量%≤Ni。 ≤15质量%,0质量%≤Al≤3质量%,0质量%≤C≤0.4质量%,其余为Fe和不可避免的杂质,成分组成满足式(a)的条件:37 <[ %Mn] + 0.3 [%Si] + 0.7 [%Cr] + 2.4 [%Ni] + 5.2 [%A] + 28 [%C] <45,且式(b):[%Ni] + 30 [% C] + 0.5 [%Mn]> 0.75 [%Cr] + 1.125 [%Si] + 2 [%Al]。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号