首页> 外国专利> Calcium Sulfoaluminate-Based Clinker Composition Used Disposal Resources Cement Composition Containing the Clinker Composition and Method for Manufacturing the Cement Composition

Calcium Sulfoaluminate-Based Clinker Composition Used Disposal Resources Cement Composition Containing the Clinker Composition and Method for Manufacturing the Cement Composition

机译:含硫铝酸钙基熟料组合物的处置资源包含熟料组合物的水泥组合物及其制造方法

摘要

The present invention relates to a calcium sulfoaluminate based clinker composition, a cement composition including the same and a method for manufacturing the cement composition, which can save natural resources and prevent environmental pollution by using industrial byproduct resources as raw material and can improve long-term strength as well as initial strength of slag based cement or general Portland cement. The calcium sulfoaluminate based clinker composition contains: 15-45 wt% of at least one selected among fluidized bed combustion ash remaining after burning petroleum coke as a fuel, fluidized bed combustion ash remaining after burning coal as a fuel and pulverized coal combustion ash in a steam power plant; 30-70 wt% of reduced slag in an electric furnace; 1-30 wt% of aluminum dross; and 1-20 wt% of gypsum. The cement composition containing the calcium aluminate based clinker according to the present invention makes an alkali component among the fluidized bed combustion ash generate alkali double salt to enhance the initial strength and makes a free lime component among the reduced slag in the electric furnace transitioned into β-C_2S mineral with high-temperature stable phase to increase the long-term strength, thereby showing excellent long-term strength as well as initial strength. In addition, the cement composition is manufactured by using industrial wastes as a raw material to save waste processing costs and manufacturing costs, and recycles wastes to save the natural resources and to prevent the environmental pollution, thereby being eco-friendly.
机译:本发明涉及一种基于硫铝酸钙的熟料组合物,包括该组合物的水泥组合物以及该水泥组合物的制造方法,其可以利用工业副产物资源作为原料来节省自然资源并防止环境污染并且可以改善长期使用。矿渣基水泥或普通硅酸盐水泥的强度以及初始强度。硫铝酸钙基熟料组合物包含:15-45 wt%的至少一种,其选自在燃烧石油焦作为燃料后残留的流化床燃烧灰,在作为燃料的煤燃烧后残留的流化床燃烧灰和在煤中的粉煤燃烧灰。蒸汽发电厂;电炉中还原渣的30-70 wt%; 1-30重量%的铝渣;和1-20wt%的石膏。根据本发明的含有铝酸钙基熟料的水泥组合物使流化床燃烧灰中的碱成分产生碱金属双盐以增强初始强度,并使电炉中的还原炉渣中的游离石灰成分转变为β。 -C_2S矿物具有高温稳定相,可提高长期强度,从而显示出优异的长期强度和初始强度。另外,水泥组合物通过使用工业废物作为原料来制造,以节省废物处理成本和制造成本,并回收废物以节省自然资源并防止环境污染,从而是生态友好的。

著录项

  • 公开/公告号KR20180014373A

    专利类型

  • 公开/公告日2018-02-08

    原文格式PDF

  • 申请/专利权人 SEWAVISION CO. LTD.;

    申请/专利号KR20160097371

  • 发明设计人 LEE BONG HAN;HAN KI SUK;JUNG JAE HYUN;

    申请日2016-07-29

  • 分类号C04B7/48;C04B14/06;C04B14/30;C04B14/36;C04B18/06;C04B18/14;C04B22/06;C04B7/02;C04B7/52;

  • 国家 KR

  • 入库时间 2022-08-21 12:40:56