The invention relates to a process for the continuous synthesis of a modified diene elastomer comprising at least one silicon atom directly connected to the elastomeric chain, comprising: a) a polymerization step by means of n reactors r1 to rn, equipped with an internal stirring system, assumed to be perfectly stirred, arranged in series, n varying from 2 to 15, preferably from 2 to 9, the reactor r1 being fed with an input solution comprising a solvent, one or more monomers, a anionic polymerization initiator selected from lithium amides and a polar agent, one or more of the reactor (s) r2 to rn optionally being further supplied by reinjection of a purified solution comprising solvent and / or monomers and / or polar agent, the temperature of each reactor ranging from 20 to 150 ° C, preferably ranging from 30 to 120 ° C and being greater than or equal to the temperature of the reactor which the p reagent immediately, the temperature of the reactor rn being greater than the reactor temperature r1, the living diene elastomer obtained having a polymolecularity index ranging from 1.1 to 1.7, b) a step of modifying the living diene elastomer obtained in the previous step by means of a functionalizing agent, coupling or starring.
机译:本发明涉及一种连续合成包含至少一个直接连接到弹性体链上的硅原子的改性二烯弹性体的方法,该方法包括:a)通过配备有内部搅拌系统的n个反应器r1至rn进行聚合步骤假定被完全搅拌,串联排列,n为2至15,优选为2至9,反应器r1被供入包含溶剂,一种或多种单体,选自酰胺化锂的阴离子聚合引发剂的输入溶液。和极性剂,反应器r2至rn中的一个或多个反应器任选地通过再注入包含溶剂和/或单体和/或极性剂的纯化溶液来进一步提供,每个反应器的温度为20至150° C,优选在30至120°C的范围内,并且大于或等于p试剂立即反应的反应器的温度,反应器的温度rn大于反应器的te在性能r1中,获得的多分子指数为1.1-1.7的活性二烯弹性体,b)通过官能化剂,偶联或加星键改性在先前步骤中获得的活性二烯弹性体的步骤。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号