Sr9−a−b−xMaMg1.5+b(PO4)7:xEu2+  formula Iwherein in formula I, said M is one or two of Ca and Ba; and 0.001≤x≤0.9, 0≤a≤1.0, 0≤b≤2.3. This orange-yellow-emitting phosphor uses a phosphate as the host material and Eu2+ ions as activation ions. The chemical properties of the phosphor are stable. The phosphor has relatively wide excitation band and emission band. And the red component in its emission spectrum is abundant, therefore, coupling the blue InGaN chip with the orange-yellow-emitting phosphor provided by this invention can obtain warm white light. The phosphor is radiation free, therefore, it will not be harmful to the environment. It is indicated by experimental results that this orange-yellow-emitting phosphor can be effectively excited by light at a wavelength of 250-500 nm and emits a wide peak at 470-850 nm, wherein the main emission peaks lie at about 523 nm and 620 nm. This preparation method is simple, and the cost is relatively low, so it is amenable to industrial production."/> Orange-yellow-emitting phosphor for LEDs, preparation method and use thereof
首页> 外国专利> Orange-yellow-emitting phosphor for LEDs, preparation method and use thereof

Orange-yellow-emitting phosphor for LEDs, preparation method and use thereof

机译:用于led的橙黄色发光荧光粉,其制备方法和用途

摘要

This invention provides an orange-yellow-emitting phosphor, the preparation method and the use thereof. This orange-yellow-emitting phosphor has a general formula represented by formula I:Sr9−a−b−xMaMg1.5+b(PO4)7:xEu2+  formula Iwherein in formula I, said M is one or two of Ca and Ba; and 0.001≤x≤0.9, 0≤a≤1.0, 0≤b≤2.3. This orange-yellow-emitting phosphor uses a phosphate as the host material and Eu2+ ions as activation ions. The chemical properties of the phosphor are stable. The phosphor has relatively wide excitation band and emission band. And the red component in its emission spectrum is abundant, therefore, coupling the blue InGaN chip with the orange-yellow-emitting phosphor provided by this invention can obtain warm white light. The phosphor is radiation free, therefore, it will not be harmful to the environment. It is indicated by experimental results that this orange-yellow-emitting phosphor can be effectively excited by light at a wavelength of 250-500 nm and emits a wide peak at 470-850 nm, wherein the main emission peaks lie at about 523 nm and 620 nm. This preparation method is simple, and the cost is relatively low, so it is amenable to industrial production.
机译:本发明提供了一种橘黄色发光的荧光粉,其制备方法及其用途。该发射橙黄色的磷光体具有由式I表示的通式:<?in-line-formulae description =“在线公式” end =“ lead”?> Sr 9-a-b-x M a Mg 1.5 + b (PO 4 7 :x Eu 2 + 公式I <? -line-formulae description =“在线公式” end =“ tail”?>其中在式I中,所述M为Ca和Ba中的一个或两个; 0.001≤x≤0.9,0≤a≤1.0,0≤b≤2.3。该发射橙黄色的磷光体使用磷酸盐作为主体材料,并使用Eu 2 + 离子作为活化离子。磷光体的化学性质是稳定的。磷光体具有相对较宽的激发带和发射带。而且,其发射光谱中的红色成分丰富,因此,将蓝色InGaN芯片与本发明提供的橙黄色发光磷光体耦合可获得温暖的白光。磷光体无辐射,因此对环境无害。实验结果表明,该橙黄色发光磷光体可以被波长为250-500 nm的光有效激发,并在470-850 nm处发射一个宽峰,其中主要发射峰位于523 nm处。 620纳米该制备方法简单,成本较低,适合工业化生产。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号