Ce3+-doped lutetium aluminum garnet (LuAG) phosphors have been successfully synthesized by a facile carbon-free sol-gel method without using any organic gelling agent. Phase transitions from gel to LuAG were well investigated by X-ray diffraction and thermal analysis. The results confirmed that a pure LuAG phase can form at around 920 °C by directly crystallizing from amorphous material. Particle size of the LuAG phosphor can be controlled by adjusting the heat treatment process; therefore, both nano and micron-scale products can be obtained and they are suitable for the fabrication of laser scintillators and white light emitting diodes, respectively. Agglomeration can be observed in the nano-sized phosphor. For the micron-sized LuAG, a two-step process was used to avoid hard agglomeration. Particles of the obtained micron-sized phosphor are uniform and well-dispersed. Luminescence properties of the phosphors were characterized. Relative intensity of the micron-sized product is comparable with commercial phosphor. ? 2014 Published by Elsevier B.V.
机译:Ce3 +掺杂的aluminum铝石榴石(LuAG)荧光粉已通过不使用任何有机胶凝剂的简便无碳溶胶-凝胶法成功合成。通过X射线衍射和热分析已很好地研究了从凝胶到LuAG的相变。结果证实,通过直接从非晶态材料结晶,可以在920°C左右形成纯LuAG相。 LuAG荧光粉的粒径可以通过调整热处理工艺来控制;因此,可以获得纳米级和微米级产品,它们分别适合于制造激光闪烁器和发白光的二极管。在纳米尺寸的磷光体中可以观察到团聚。对于微米级的LuAG,使用两步过程来避免硬团聚。所获得的微米级磷光体的颗粒均匀且分散良好。表征了磷光体的发光性质。微米级产品的相对强度与商业荧光粉相当。 ? 2014由Elsevier B.V.发布

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号