METHOD FOR FORMING A FILM COMPRISING NANOCELLULOSE
METHOD FOR FORMING A FILM COMPRISING NANOCELLULOSE
展开▼
机译:形成包含纳米纤维素的膜的方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
A method of forming a film comprising nanocellulose having an Oxygen Transmission Rate (OTR) value in the range of 0.1 to 300 cc/m2/24 h at 38° C. and 85% relative humidity (RH), and having a basis weight in the range of in the range of 0.1 to 45 g/m2 wherein the method comprises the steps of; providing a suspension comprising nanocellulose, forming at least one layer of a web or a film from said suspension; drying said formed web or film to a dry content of at least 65 weight-%, wherein said method further comprises the steps of; treating at least one side of said dewatered and dried web or film with ultra violet (UV) or electron beam (EB) irradiation; and wherein at least one cooling step is provided in connection with or after the UV or EB treatment step.
展开▼
机译:一种形成膜的方法,该膜包括在38℃,相对湿度(RH)为85%的情况下,氧气透过率(OTR)值在0.1至300 cc / m 2 Sup> / 24 h范围内的纳米纤维素。 ),并且具有在0.1至45 g / m 2 Sup>范围内的基重,其中该方法包括以下步骤:提供包含纳米纤维素的悬浮液,其由所述悬浮液形成至少一层网或薄膜。将所述成形的幅材或薄膜干燥至至少65重量%的干含量,其中所述方法还包括以下步骤:用紫外线(UV)或电子束(EB)辐射处理所述脱水和干燥的幅材或薄膜的至少一侧;并且其中在UV或EB处理步骤之后或之后提供至少一个冷却步骤。
展开▼