A first method is disclosed for forming a tubular reinforcement that comprises the steps of: providing a 7xxx aluminum tube, heating tube to at least 450° C. and water quenching the tube in less than or equal to 20 seconds after heating. All of the forming processes on the tube are then completed from within 1 to 8 hours of quenching. A second method for forming a tubular reinforcement is disclosed that comprises the steps of providing a 7xxx-O temper aluminum tube and forming the tube into a predetermined shape. The tube in then heated the tube to at least 450° C. and quenched the tube with water or air in a hydroforming die just prior to or while hydroforming the tube.
机译:公开了用于形成管状加强件的第一方法,该方法包括以下步骤:提供7xxx铝管,将加热管加热到至少450°C,并在加热后少于或等于20秒的时间内用水淬灭该管。然后在淬火的1到8个小时内完成管子上的所有成型过程。公开了用于形成管状加强件的第二种方法,该方法包括以下步骤:提供7xxx-O回火铝管并将管形成为预定形状。然后,将管加热到至少450℃,并在将其液压成形之前或同时在液压成形模具中用水或空气将其淬火。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号