Production method of environment-friendly water-repellent synthetic leather using non-fluorine water repellent agent

机译:使用无氟憎水剂的环保型憎水合成革的生产方法

摘要

The present invention relates to a method for manufacturing environmentally-friendly water-repellent synthetic leather using a non-fluoride water-repelling agent, which is environmentally-friendly, is harmless to humans, and maximizes water repellency. According to the present invention, the method comprises: an impregnation step of impregnating a polyester tricot napped fabric in a mixed water repellent solution for impregnation which includes a water-dispersed polyurethane and the non-fluoride water-repelling agent; a mangling step of mangling the fabric impregnated in the mixed water repellent solution for impregnation to adjust a moisture content at 40 to 80%; a silver layer forming step of coating a mixed water repellent solution for coating, which includes the water-dispersed polyurethane and the non-fluoride water-repelling agent, on the fabric completing the mangling step; a drying step of drying the fabric completing the silver layer forming step at 90 to 100°C for 2 to 4 min by hot air through a dryer; and a curing step of curing the fabric completing the drying step at 140 to 150°C for 4 to 6 min in a curing apparatus.
机译:本发明涉及一种使用无氟拒水剂的环保拒水合成革的制造方法,该方法是环保的,对人体无害,并具有最大的拒水率。根据本发明,该方法包括:将聚酯经编织物成网的织物浸渍在包括水分散的聚氨酯和非氟化憎水剂的用于混合的憎水混合溶液中的浸渍步骤;整理步骤,对浸渍在混合防水溶液中的织物进行浸渍以将水分含量调节为40-80%。银层形成步骤,其在织物上涂覆用于混合的疏水性溶液,该混合的疏水性溶液包括水分散的聚氨酯和非氟化性疏水剂,从而完成所述上浆步骤;干燥工序是通过干燥机用热风在90〜100℃下干燥完成银层形成工序的织物2〜4分钟的干燥工序。固化步骤是将织物在固化装置中在140至150℃下完成干燥步骤4至6分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号