Eco-friendly water-repellent synthetic leather using non-fluorine water repellent

机译:使用无氟拒水剂的环保拒水合成革

摘要

The present invention relates to an environmentally-friendly water-repellent synthetic leather using a non-fluoride water-repelling agent, which is environmentally-friendly, is harmless to humans, and maximizes water repellency. According to the present invention, the environmentally-friendly water-repellent synthetic leather comprises: a polyester tricot napped fabric layer; a non-fluoride water-repelling agent impregnated layer formed by impregnating the napped fabric in a mixed water repellent solution for impregnation which includes a water-dispersed polyurethane and the non-fluoride water-repelling agent; and a silver layer formed by coating a mixed water repellent solution for coating, which includes the water-dispersed polyurethane and the non-fluoride water-repelling agent, on surfaces of the napped fabric layer and the non-fluoride water-repelling agent impregnated layer, wherein the non-fluoride water-repelling agent impregnated layer and the silver layer are dried at 90 to 100°C for 2 to 4 min by hot air and then are cured at 140 to 150°C for 4 to 6 min in a curing apparatus.
机译:本发明涉及一种使用无氟拒水剂的环保拒水合成革,它是环保的,对人体无害,并具有最大的拒水率。根据本发明,该环保型疏水性合成皮革包括:聚酯经编短毛绒织物层;和通过将绒头织物浸渍在用于浸渍的混合防水溶液中而形成的非氟化防水剂浸渍层,其包括水分散的聚氨酯和非氟化防水剂;通过在绒头织物层和非氟化防水剂浸渍层的表面上涂覆包括水分散的聚氨酯和非氟化防水剂的混合防水溶液而形成的银层。 ,其中将所述非氟防水剂浸渍层和银层通过热空气在90至100℃下干燥2至4分钟,然后在140至150℃下固化4至6分钟。仪器。

著录项

  • 公开/公告号KR20200053155A

    专利类型

  • 公开/公告日2020-05-18

    原文格式PDF

  • 申请/专利权人 HYUN DAE SIK MO CO. LTD.;

    申请/专利号KR20180136394

  • 发明设计人 KIM SUNG WOO;HUH HAN CHANG;YI SEUNG DONG;

    申请日2018-11-08

  • 分类号D06N3;D06M11/83;D06N3/14;

  • 国家 KR

  • 入库时间 2022-08-21 11:07:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号