Eco-friendly water-repellent synthetic leather using non-fluorine water repellent

机译:使用无氟拒水剂的环保拒水合成革

摘要

The present invention relates to an eco-friendly water-repellent synthetic leather using a non-fluorine water-repellent agent, and is eco-friendly and harmless to the human body, and at the same time, a polyester tricot brushed fabric layer, a water-dispersible polyurethane and non-fluorine in the brushed fabric layer, to maximize water repellency. A non-fluorine water-repellent impregnation layer formed by impregnating a water-repellent mixture for impregnation containing a water-repellent agent, and a silver layer formed by coating a water-repellent mixture for coating on the surfaces of the brushed fabric layer and the non-fluorine-free water-repellent impregnation layer, and the non-fluorine water-repellent The impregnated layer and the silver layer are hot air dried at 90°C to 110°C for 2 to 4 minutes and then cured in a curing machine at 140°C to 150°C for 4 to 6 minutes.
机译:本发明涉及一种使用非氟防水剂的环保防水合成革,对人体无害且环保,同时还涉及一种涤纶经编拉丝织物层,一种在拉绒织物层中具有水分散性聚氨酯和非氟,可最大程度地提高拒水性。通过浸渍包含疏水剂的用于浸渍的疏水混合物而形成的非氟疏水浸渍层,以及通过在涂刷的织物层和织物的表面上涂覆用于涂布的疏水混合物而形成的银层。无氟防水浸渍层和无氟防水浸渍层和银层在90℃至110℃下热风干燥2至4分钟,然后在固化机中固化在140°C至150°C下放置4至6分钟。

著录项

  • 公开/公告号KR102151967B1

    专利类型

  • 公开/公告日2020-09-04

    原文格式PDF

  • 申请/专利权人 (주)현대식모;

    申请/专利号KR20180136394

  • 发明设计人 김성우;허한창;이승동;

    申请日2018-11-08

  • 分类号D06N3;D06M11/83;D06N3/14;

  • 国家 KR

  • 入库时间 2022-08-21 11:03:52

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号