摘要

The effects of calcination temperature, Cu source and co-template contents on the activity and hydrothermal stability of Cu-SAPO-34 catalysts prepared by the one-pot hydrothermal synthesis method were investigated. Appropriate calcination temperature was important for the deNOx activity of Cu-SAPO-34 catalyst. The amount of Cu source and co-template in the resulting gel could impact the Cu loading and the crystallization of the final Cu-SAPO-34. Preferably, hydrothermal treatment of the Cu-SAPO-34 catalyst with Cu loading ca. 3.44% at 750 degrees C for 16 h increased the NH3-SCR activity slightly due to migration of CuO to isolated Cu2+ and the maintenance of the crystallinity as well as the acidity. Moreover, the catalyst aged at 800 degrees C for 16 h maintained >90% NOx conversion from 225 to 400 degrees C, and the crystallinity, active Cu2+ species and acidity in Cu-SAPO-34 were not destroyed completely after such harsh treatment. Meanwhile, kinetic analysis over fresh and aged Cu-SAPO-34 samples were conducted and the conclusion were in agreement with the NH3-SCR tests, H-2-TPR and NH3-TPD results. (C) 2016 Elsevier B.V. All rights reserved.
机译:研究了一锅水热合成法制备的Cu-SAPO-34催化剂的焙烧温度,Cu源和共模板含量对催化剂活性和水热稳定性的影响。适当的煅烧温度对于Cu-SAPO-34催化剂的脱硝活性至关重要。所得凝胶中的铜源和共模板的数量可能会影响铜的负载量和最终Cu-SAPO-34的结晶。优选地,以Cu负载约200对Cu-SAPO-34催化剂进行水热处理。在750摄氏度下反应了3.44%,持续16 h,由于CuO迁移到分离的Cu2 +上并保持了结晶度和酸度,NH3-SCR活性略有提高。此外,在800摄氏度下老化16小时的催化剂在225至400摄氏度之间保持> 90%的NOx转化率,经过这种苛刻的处理后,Cu-SAPO-34的结晶度,活性Cu2 +种类和酸度没有被完全破坏。同时,对新鲜和老化的Cu-SAPO-34样品进行了动力学分析,其结论与NH3-SCR试验,H-2-TPR和NH3-TPD结果相吻合。 (C)2016 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号