Effect of BN content on microstructures, mechanical and dielectric properties of porous BN/Si_3N_4 composite ceramics prepared by gel casting

机译:BN含量对凝胶浇铸制备的多孔BN / Si_3N_4复合陶瓷微观结构,力学和介电性能的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Porous BN/Si_3N_4 composite ceramics with different BN contents have been fabricated by gel casting. The rheological behaviors of the suspensions, microstructure, mechanical properties, dielectric properties and critical temperature difference of thermal shock (ΔT_C) of porous BN/Si_3N_4 composite ceramics with different BN contents were investigated. With BN contents increasing, the mechanical properties of the porous BN/Si_3N_4 composite ceramics were partially declined, but the dielectric properties and thermal shock resistances were enhanced at the same time. For the porous Si_3N_4 ceramic without BN addition, the porosity, flexural strength, dielectric constant and critical temperature difference were 48.1%, 128 MPa, 4.1 and 395 °C, while for the 10 vol% BN/Si_3N_4 porous composite ceramics, they were 49.4%, 106.6 MPa, 3.8, and 445 °C, respectively. The overall performance of the obtained porous BN/Si_3N_4 composite ceramics indicated that it could be one of the ideal candidates for high-temperature wave-transparent applications.
机译:通过凝胶浇铸制备了不同BN含量的多孔BN / Si_3N_4复合陶瓷。研究了不同BN含量的多孔BN / Si_3N_4复合陶瓷的悬浮液的流变行为,微观结构,力学性能,介电性能和热冲击临界温差(ΔT_C)。随着BN含量的增加,多孔BN / Si_3N_4复合陶瓷的力学性能有所下降,但介电性能和抗热震性同时提高。对于不添加BN的多孔Si_3N_4陶瓷,其孔隙率,抗弯强度,介电常数和临界温差分别为48.1%,128 MPa,4.1和395°C,而对于10 vol%的BN / Si_3N_4多孔复合陶瓷,其孔隙率为49.4%。 %,106.6 MPa,3.8和445°C。所获得的多孔BN / Si_3N_4复合陶瓷的整体性能表明,它可能是高温波透明应用的理想候选者之一。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号