This paper deals with the determination of color change for oak, birch and pine wood. Color changes were measured on native and thermally modified wood. The thermal modification was carried out at four different temperatures: 160 degrees C, 180 degrees C, 210 degrees C and 240 degrees C. Color changes were evaluated according to CIE L*a*b* method by parameters L*, a*, b* and Delta E*. After the heat treatment, the lightness L* of wood was reduced for all wood species. The a* values had a similar character for oak and birch wood, while the values of pine showed an opposite character. Increasing the temperature resulted in a decrease in the values of the parameter b* for oak and birch wood. However, pine wood achieved the highest b* values during thermal modification at a temperature of 160 degrees C. Further increases in temperature led to a gradual lowering of these values. The overall color change Delta E* gradually grew with the increase in temperature for oak and birch, while pine had the highest value at a temperature of 160 degrees C.
机译:本文涉及确定橡木,桦木和松木的颜色变化。在天然和热改性木材上测量颜色变化。在四个不同的温度下进行热改性:160摄氏度,180摄氏度,210摄氏度和240摄氏度。根据CIE L * a * b *方法通过参数L *,a *,b评估颜色变化*和Delta E *。热处理后,所有木材种类的木材亮度L *均降低。橡木和桦木的a *值具有相似的特征,而松木的a *值具有相反的特征。温度升高导致橡木和桦木的参数b *值降低。然而,松木在160℃的温度下的热改性期间达到了最高的b *值。温度的进一步升高导致这些值逐渐降低。随着橡木和桦木温度的升高,总的颜色变化量Delta E *逐渐增加,而在160摄氏度的温度下松木的最高值变化最大。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号