STRUCTURAL CHARACTERIZATION OF LIGNIN EXTRACTED WITH ALKALINE HYDROGEN PEROXIDE FROM FURFURAL RESIDUE

机译:糠醛残渣中碱性过氧化氢提取的木质素的结构表征

获取原文
获取原文并翻译 | 示例
           

摘要

Lignin from furfural residue was extracted with alkaline hydrogen peroxide at different temperatures and times. The structural features of lignins were characterized by elemental analysis, GPC, FT-IR, H-1 NMR, C-13 NMR and Py-GC/MS. Results showed that the yield of lignin increased with the increase of reaction time and temperature. The maximum lignin yield of 41.4% (corresponding to the original lignin) was achieved by extraction at 80 degrees C for 3 h. The average-molecular weight (M-w) of the extracted lignins (780-850) was about 1/4 of that of the MWL (milled wood lignin) of furfural residue (2890), which indicated a severe degradation of furfural residue lignin under the treatment. Py-GC/MS analysis indicated that the major unit in lignins was p-hydroxycinnamyl (H), together with lower amounts of syringyl (S) and guaiacyl (G) units. The relative molar content of the H unit in the extracted lignins increased, as compared to MWL.
机译:用碱性过氧化氢在不同的温度和时间下提取糠醛残渣中的木质素。通过元素分析,GPC,FT-IR,H-1 NMR,C-13 NMR和Py-GC / MS表征木质素的结构特征。结果表明,随着反应时间和温度的升高,木质素的得率增加。通过在80摄氏度下萃取3小时,木质素的最大产率为41.4%(相当于原始木质素)。提取的木质素(780-850)的平均分子量(Mw)约为糠醛残留物(2890)的MWL(碾碎的木质素)的1/4,表明糠醛残留木质素在此条件下会严重降解。治疗。 Py-GC / MS分析表明,木质素中的主要单位是对羟基肉桂基(H),以及较少的丁香基(S)和愈创木基(G)单位。与MWL相比,提取的木质素中H单元的相对摩尔含量增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号