The influence of thickness ratio (TR) on the formability and forming limit diagram (FLD) of tailor welded blanks (TWB) obtained by pulsed Nd:YAG laser welding of St12 steel sheets are studied. Steel sheets with thicknesses of 0.5, 0.8 and 1.0 mm were combined to form TWBs of different thickness ratios of 2 (1.0/0.5 mm), 1.6 (0.8/0.5 mm) and 1.25 (1.0/0.8 mm). Limit thickness ratio (LTR) is introduced as a new useful factor for prediction of forming limit of TWB. Results of this research show that by increasing the difference of thickness ratio of TWB and LTR, formability and the level of FLD will decrease. In addition, effects of thickness ratio of TWB on the punch's load-displacement, limit dome height (LDH) and weld line movement are studied. By increasing the thickness ratio, the LDH decreases and some defects such as weld line movement and wrinkling increase. The experimental findings of this study show that the thickness ratio of TWB can effect on the position of fracture in TWB products.
机译:研究了厚度比(TR)对通过脉冲Nd:YAG激光焊接St12钢板获得的拼焊板(TWB)的可成形性和成形极限图(FLD)的影响。合并厚度为0.5、0.8和1.0毫米的钢板,以形成厚度比分别为2(1.0 / 0.5毫米),1.6(0.8 / 0.5毫米)和1.25(1.0 / 0.8毫米)的TWB。引入极限厚度比(LTR)作为预测TWB成形极限的新有用因素。研究结果表明,通过增加TWB和LTR的厚度比之差,可成形性和FLD含量将降低。此外,研究了TWB的厚度比对冲头的载荷-位移,极限拱顶高度(LDH)和焊缝运动的影响。通过增加厚度比,LDH减少,并且某些缺陷(如焊缝移动和起皱)增加。这项研究的实验结果表明,TWB的厚度比可以影响TWB产品中的断裂位置。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号