Preparation of Fe_(65)Co_(10)Ga_5P_(12)C_4B_4 Bulk Glassy Alloy with Good Soft Magnetic Properties by Spark-Plasma Sintering of Glassy Powder

机译:玻璃粉末的放电等离子烧结制备具有良好软磁性能的Fe_(65)Co_(10)Ga_5P_(12)C_4B_4大块玻璃态合金

获取原文
获取原文并翻译 | 示例
       

摘要

With the aim of developing a large size bulk glassy Fe-based alloy with good soft magnetic properties by the powder metallurgy technique, we have applied the spark-plasma sintering technique to a Fe_(65)Co_(10)Ga_5P_(12)C_4B_4 glassy alloy powder with a large supercooled liquid region of 50K before crystallization. The existence of the supercooled liquid region enabled us to form a large size bulk glassy alloy of 20mm in diameter and 5mm n thickness with a high relative density of 99 percent. The resulting bulk glassy alloy exhibits good soft magnetic properties, i.e., 1.20T for saturation magnetization, 14A/m for coercive force and 6000 for maximum permeability. The good soft magnetic properties for the multicomponent Fe-based bulk alloy are attributed to the combination of the high relative density and the maintenance of the single glassy structure. The success of forming the large size bulk glassy alloy with good soft magnetic properties by the powder metallurgy techniques is promising for future use as practical soft magnetic materials.
机译:为了通过粉末冶金技术开发出具有良好软磁性能的大尺寸块状玻璃态铁基合金,我们将火花等离子体烧结技术应用于Fe_(65)Co_(10)Ga_5P_(12)C_4B_4玻璃态结晶前具有50K大过冷液体区域的合金粉末。过冷液体区域的存在使我们能够形成直径为20mm,厚度为5mm的大块体玻璃状合金,相对密度为99%。所得的块状玻璃态合金具有良好的软磁性能,即饱和磁化强度为1.20T,矫顽力为14A / m,最大磁导率为6000。多组分铁基块状合金的良好软磁性能归因于高相对密度和单一玻璃态结构的维持。通过粉末冶金技术成功地形成具有良好软磁性能的大块体玻璃状合金,有望在将来用作实用的软磁材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号