首页> 外国专利> FE-BASED SOFT MAGNETIC GLASSY ALLOY MATERIAL

FE-BASED SOFT MAGNETIC GLASSY ALLOY MATERIAL

机译:基于FE的软磁性玻璃合金材料

摘要

The invention is related to an Fe based alloy material, suitable for producing a soft magnetic glassy alloy product, a product produced thereof and a method for producing such a product. The product can be a master alloy product obtained after a first melting step starting from suitably selected starting materials, or it can be a final soft magnetic glassy alloy product obtained after a further step of melting the master alloy. The alloy material of the invention comprises : ⋅ C between 1.4wt% and 2.2wt% ⋅ Si between 0.9wt% and 1.35wt% ⋅ B between 0.43wt% and 0.65wt% ⋅ P between 5wt% and 7.5wt% ⋅ Mo between 0.9wt% and 9.2wt% ⋅ Mn between 0.05wt% and 0.6wt%, ⋅ O up to 0.3wt%, ⋅Al up to 0.1wt%, ⋅ S up to 0.05wt%, ⋅ Ti up to 0.45wt%, ⋅ Cr up to 0.3wt%, ⋅ Cu up to 0,25wt% or Cu between 0.25wt% and 0.8wt%, the balance being Fe and incidental impurities. A Fe-based soft magnetic glassy product according to the invention can be produced starting from non-pure starting materials.
机译:本发明涉及一种适用于生产软磁性玻璃态合金产品的铁基合金材料,其生产的产品以及生产这种产品的方法。该产物可以是在从合适选择的起始原料开始的第一熔融步骤之后获得的中间合金产物,或者可以是在进一步熔融该中间合金的步骤之后获得的最终软磁玻璃态合金产物。本发明的合金材料包括:·1.4wt%至2.2wt%之间的C·0.9wt%至1.35wt%之间的Si·0.43wt%至0.65wt%之间的B·5wt%至7.5wt%之间的P·Mo Mn在0.05wt%和0.6wt%之间为0.9wt%和9.2wt%⋅Mn,∙O高达0.3wt%,⋅Al高达0.1wt%,⋅S高达0.05wt%,⋅Ti高达0.45wt%, ·Cr最高可达0.3wt%,⋅Cu最高可达0.25%wt,或Cu含量在0.25wt%至0.8wt%之间,其余为Fe和附带的杂质。可以从非纯起始原料开始生产根据本发明的Fe基软磁性玻璃状产品。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号