With the aim of developing a large size Fe-based bulk glassy core with good soft magnetic properties by the powder metallurgy technique, we have applied the spark-plasma sintering technique to a Fe_(65)Co_(10)Ga_5P_(12)C_4B_4 glassy alloy powder with a large supercooled liquid region of 50 K before crystallization. The existence of the supercooled liquid region enabled us to form a large size glassy alloy bulk of 20 mm in diameter and 5 mm in thickness with a high relative density of 99.7%. The resulting bulk glassy magnetic core of 20 mm in outer diameter, 10mm in inner diameter and 4mm in thickness exhibits good soft magnetic properties, i.e. 1.20T for saturation magnetization, 6 A/m for coercive force and 8900 for maximum permeability. The good soft magnetic properties for the multicomponent Fe-based bulk glassy core are attributed to the combination of the high relative density and the maintenance of the single glassy structure.
机译:为了通过粉末冶金技术开发出具有良好软磁性能的大尺寸铁基块状玻璃核,我们将火花等离子体烧结技术应用于Fe_(65)Co_(10)Ga_5P_(12)C_4B_4玻璃态结晶前具有50 K的大过冷液体区域的合金粉末。过冷液体区域的存在使我们能够形成直径为20毫米,厚度为5毫米的大尺寸玻璃态合金块,相对密度为99.7%。所得的大块玻璃状磁芯的外径为20mm,内径为10mm,厚度为4mm,具有良好的软磁性能,即饱和磁化强度为1.20T,矫顽力为6A / m,最大磁导率为8900。多组分铁基块状玻璃核的良好软磁性能归因于高相对密度和单一玻璃态结构的维持。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号