In the traditional hot forging, the temperature of the billet is heated to the forming range, and the die does not need to be heated or only slightly preheated. In isothermal forging, the temperature of the die needs to be heated to the same as that of the billet and kept constant during forging. This paper proposes a new method, which is to control the die temperature to a certain extent higher than that of the billets during the hot forming process. The method was verified by the upsetting process. The finite element analysis and upsetting experiment were carried out, and the method result was compared with the ordinary upsetting method and isothermal upsetting method. It has been found that this method can significantly improve the bulging phenomenon during upsetting. The KD value was introduced to characterize the bulging degree of the forging. Increasing the die temperature has a significant inhibiting effect on the instability of large-size billets during upsetting. By this method, when the billet is heated to 380 degrees C and the die temperature is stabilized at 405 degrees C, the upsetting of 2024 aluminum alloy with an aspect ratio of 3.7 can be realized. This method has not been reported to our knowledge.
机译:在传统的热锻中,将坯料的温度加热到成型范围,模具不需要加热或只需稍微预热即可。在等温锻造中,模具的温度需要加热到与坯料相同的温度,并在锻造过程中保持恒定。本文提出了一种新的方法,即在热成型过程中将模具温度控制在一定程度上高于坯料。通过翻转过程验证了该方法的有效性。进行了有限元分析和镦粗实验,并将方法结果与普通镦粗法和等温镦粗法进行了对比。研究发现,该方法可以显著改善镦粗过程中的鼓包现象。引入KD值来表征锻件的膨胀程度。提高模具温度对大尺寸钢坯在镦粗过程中的不稳定性有显著的抑制作用。通过这种方法,当钢坯加热到380°C,模具温度稳定在405°C时,可以实现长径比为3.7的2024铝合金的镦粗。据我们所知,这种方法尚未报告。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号