Information about con-elation of material properties parameters (i.e., crystallite and particle sizes) and photocatalytic activity of tungsten trioxide (WO3) particles are still lacking. For this reason, the purpose of this study was to synthesize WO 3 particles with controllable crystallite (from 18 to 50 nm) and particle sizes (from 58 to 677 nm) using a spray-pyrolysis method and to investigate correlation of crystallite/particle size and photocatalytic activity. To gain control of crystallite/particle size, synthesis temperature (120-1300°C) and initial precursor concentration (2.5-15 mmollL) were investigated, which were then compared with the proposal of the particle formation mechanism. The results showed that both crystallite and particle sizes played an important role in photocatalytic activity. In this research, the optimum condition to produce the highest photocatalytic performance of WO3 particles was at the temperature of 1200°C (crystallite size: 25 nm), and initial concentration of 10 mmollL (particle size: 105 nm).
机译:仍然缺乏有关材料性能参数(即微晶和粒度)的确定和三氧化钨(WO3)颗粒的光催化活性的信息。因此,本研究的目的是使用喷雾热解法合成具有可控晶体(18至50 nm)和粒径(58至677 nm)的WO 3颗粒,并研究晶体/粒径的相关性和光催化活性。为了控制微晶/颗粒尺寸,研究了合成温度(120-1300°C)和初始前体浓度(2.5-15 mmollL),然后将其与颗粒形成机理的建议进行了比较。结果表明,微晶和粒径在光催化活性中都起着重要作用。在这项研究中,产生最高WO3颗粒光催化性能的最佳条件是在1200°C(微晶尺寸:25 nm)的温度和10 mmollL(颗粒尺寸:105 nm)的初始浓度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号