Radiant tubes of topping furnaces have to ensure safe operation during long time under critical conditions for material stability, due to the combined effects of environment and creep. In this paper, radiant tubes made of ASTM 335 grade P5 were inspected after more than 200,000 h of service, in order to assess any damaging conditions incompatible for safe operating. Visual inspection of the external surfaces and diameter ultrasonic measurements were performed during a scheduled shutdown of the furnace: the most critical sections were investigated 'in situ' by means of replica method and Vickers hardness surveys. Tubes were put out of service when their external surface showed burns caused by flame impingement and thickness was reduced to unacceptable values. Specimens cut from two decommissioned tubes were characterised by means of tension test and accelerated creep test: their residual life was calculated numerically taking into account also the effects of wall thickness reduction.
机译:由于环境和蠕变的组合效果,在长期以来,顶部炉子的辐射管必须在长时间内确保安全操作。 在本文中,经过200,000小时的服务后,由ASTM 335级P5制成的辐射管,以评估不兼容的任何用于安全操作的破坏性条件。 在炉子的预定关闭期间进行外表面和直径超声测量的目视检查:通过复制方法和维氏硬度调查,“原位”研究了最关键的部分。 当其外表面向火焰冲击引起的烧伤时,将管子放入服务中,厚度降低到不可接受的值。 通过张力试验和加速蠕变试验表征从两个退役管中切割的标本:它们的剩余寿命在数值上考虑了壁厚减少的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号