Characterization of the boron layer formed by pack boronizing of binary iron-niobium alloys

机译:用二元铁 - 铌合金包装硼化硼层的表征

获取原文
获取原文并翻译 | 示例

摘要

In this study, Fe-1Nb, Fe-5Nb and Fe-10Nb (at.-%) binary alloys were boronized by the pack boronizing method at 950 degrees C for 3 h. The effect on the boride layer of the increasing niobium amount in pure the iron was experimentally investigated. After boron treatment, microstructural changes occurring on the surfaces of the coated alloys were examined by SEM, EDS and XRD analysis. A microhardness test analysis was applied to the coated alloys. Typical saw tooth morphologies were present in all coated alloys. The increasing niobium amount in the pure iron suppressed the appearance of the saw tooth morphologies. In addition, the microhardness of the boron layers was much higher than that of the base metal.
机译:在本研究中,通过包装硼化方法在950℃下将Fe-1NB,Fe-5NB和Fe-10Nb(At.-%)二元合金硼化了3小时。 实验研究了对纯铁中增加铌量的硼化物层的影响。 在硼处理之后,通过SEM,EDS和XRD分析检查涂覆合金表面上发生的微观结构变化。 将显微硬度试验分析应用于涂覆合金。 在所有涂覆的合金中存在典型的锯齿形态。 纯铁中的铌量增加抑制了锯齿形态的外观。 此外,硼层的显微硬度远高于基础金属的微硬度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号