首页> 外文期刊>International Journal of Pressure Vessels and Piping >Treatment of constraint in BS 7910:2013, ISO 27306 and DNVGL-RP-F108
【24h】

Treatment of constraint in BS 7910:2013, ISO 27306 and DNVGL-RP-F108

机译:对BS 7910:2013,ISO 27306和DNVGL-RP-F108的约束治疗

获取原文
获取原文并翻译 | 示例
           

摘要

Annex N of BS 7910:2013 (`Guide to methods for assessing the acceptability of flaws in metallic structures') describes two procedures for allowing for constraint effects in fracture assessment. One (Procedure I) is based on modifying the Failure Assessment Line (FAL) to account for constraint, the other (Procedure II) on modifying the failure assessment point. They are intended to be used in conjunction with the main fracture assessment procedures (Clause 7) 'to estimate any increase in reserve factors likely to arise under conditions of low constraint.' This paper addresses the origins of Annex N and illustrates its application to the assessment of a pair of plain steel wide plate specimens containing through-thickness cracks, which failed by brittle cleavage. It is shown that the expected advantages of the method (reduction in excessive conservatism without jeopardising safety) may be offset by a need to define the fracture toughness of the specimens in a more conservative manner and/or by carrying out many more tests than is currently considered acceptable.
机译:BS 7910:2013的附件n(“金属结构中缺陷可接受性的方法指南”)描述了两个允许在骨折评估中产生约束效应的方法。一个(程序I)基于修改失败评估行(FAL)来解释约束,另一个(程序II)修改失败评估点。它们旨在与主要骨折评估程序(第7条)结合使用,以估计在低约束条件下可能出现的储备因素的任何增加。本文涉及附件N的起源,并说明其在评估含有厚度裂缝的一对普通钢宽板样品的应用,该试验失效,该裂缝失效。结果表明,该方法的预期优势(在没有危及安全性的情况下减少过度保守),可以抵消需要以更保守的方式定义样品的断裂韧性和/或通过当前进行更多的测试被认为是可接受的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号