The marble industry generates enormous amounts of waste every year, whose incorrect management can lead to environmental problems. The Circular Economy model can provide an effective solution to this issue, an aspect that has been addressed in this research. The suitability of a marble sludge generated in the ornamental rock industry of Andalusia (Spain) has been assessed as raw material in ceramic bricks. Mixtures containing a clayey base and 0, 2.5, 5, 7.5, and 10?wt% of marble powder have been shaped into 60?×?30?×?10-mm3 prismatic specimens and sintered at 950?°C in a muffle. The main technological properties of the bricks related to color, shrinkage, porosity, water absorption, suction, and compressive strength have been determined. The addition of marble sludge has fostered the development of a lighter color, together with a significant increase of the open porosity. This aspect has implied, on the one hand, higher water absorption and suction results and, on the other hand, a decrease of the density and the mechanical strength. The correlations obtained after applying Shapiro-Wilk normality tests and r Pearson coefficients endorse the clear relationship between the addition of marble powder and the abovementioned effects on the technological properties of the sintered bricks. All the measured properties fully meet the brick standardized requirements, which would indicate that the recycling of marble wastes could be a promising alternative to obtain eco-friendly lightweight ceramic materials.
机译:大理石产业每年产生大量的浪费,其管理不正确会导致环境问题。循环经济模型可以为此问题提供有效的解决方案,这项问题已经解决了这一问题。在安达卢西亚(西班牙)观赏岩石工业中产生的大理石污泥的适用性已被评估为陶瓷砖的原料。含有粘土基和0,2.5,5,7.5和10·wt%的大理石粉末的混合物已经成形为60?×30?×10-mm 3棱柱标本,并在一个muffle中在950℃下烧结。已经确定了与颜色,收缩,孔隙率,吸水,抽吸和抗压强度相关的砖的主要技术特性。大理石污泥的添加促使开发较轻的颜色,以及开放孔隙的显着增加。这方面暗示了一方面,较高的吸水性和抽吸结果,另一方面,密度和机械强度的降低。在施加Shapiro-wilk正常性测试和R Pearson系数之后获得的相关性通过基于大理石粉末和上述对烧结砖的技术性质的上述作用而获得的清晰关系。所有测量的属性完全满足砖标准化要求,表明大理石废物的回收可能是获得环保轻质陶瓷材料的有希望的替代方案。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号