The reaction between Fe-Mn-Si alloy and MnO-SiO2-FeO oxide in the solid state has been investigated using the diffusion couple by some of the authors [1]. In their previous work, the diffusion couple was preheated at 1673K for 10min to ensure a good contact between the alloy and the oxide. However, to observe the solid state reaction by the heat treatment at 1473K, the influence of the heating at 1673K was not negligible. In this study, new method to melt the oxide at 1673K to produce diffusion couple was developed and the solid state reaction at 1473K was clarified by minimizing the influence of heating at 1673K.
机译:一些作者已经使用扩散对研究了Fe-Mn-Si合金与MnO-SiO2-FeO氧化物之间的固态反应[1]。在他们以前的工作中,将扩散对在1673K下预热10分钟,以确保合金与氧化物之间的良好接触。然而,为了观察通过在1473K下的热处理的固态反应,在1673K下的加热的影响不可忽略。在这项研究中,开发了一种新的方法来熔化1673K处的氧化物以产生扩散对,并通过最小化1673K处的加热影响来澄清1473K处的固态反应。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号