Highly conductive and transparent single-walled carbon nanotube thin films fabricated by gel coating

机译:凝胶涂层制备的高导电透明单壁碳纳米管薄膜

获取原文
获取原文并翻译 | 示例

摘要

Transparent and conductive single-walled carbon nanotube (SWCNT) films were fabricated through gel coating. A gel was formed by directly dispersing a large amount of SWCNTs in a liquid nonionic surfactant like polyoxyethylene (12) tridecyl ether without a solvent by mechanical grinding and subsequent ultrasonication. SWCNT films were obtained by coating the gels on glass substrates and subsequently removing the surfactant through heating. The SWCNT films became very thin and transparent after heating at a temperature between 480 and 520 ℃. They exhibited good uniformity and a high transmittance-to-sheet resistance ratio which is attributed to the long SWCNTs dispersed in the gels. Films with a sheet resistance of around 250 Ω □~(-1) at 80% transmittance were obtained. The films can be easily transferred from rigid substrates like glass to flexible polymer substrates like polyethylene terephthalate.
机译:通过凝胶涂层制备了透明导电单壁碳纳米管(SWCNT)薄膜。通过机械研磨和随后的超声处理,将大量的SWCNT直接分散在液态非离子表面活性剂(如聚氧乙烯(12)十三烷基醚)中而无需溶剂,即可形成凝胶。通过将凝胶涂覆在玻璃基板上,然后通过加热除去表面活性剂来获得SWCNT膜。在480至520℃的温度下加热后,SWCNT薄膜变得非常薄和透明。它们表现出良好的均匀性和高的透光率/薄层电阻比,这归因于分散在凝胶中的长SWCNT。得到在80%透射率下的薄层电阻为约250Ω□〜(-1)的膜。可以容易地将膜从诸如玻璃的刚性基材转移至诸如聚对苯二甲酸乙二醇酯的柔性聚合物基材。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号