Immobilized enzymes are used as biocatalysts for analytical purposes in diagnostics and for preparative purposes in large scale industrial processes. Immobilization can increase the half-life, improve the stability, and increase the catalytic activity of an enzyme. It facilitates the separation and recovery of the catalyst from the reaction products, and allows for multiple use of the biocatalysts. Graphene oxide nanosheets were decorated with superparamagnetic iron oxide nanoparticles (SPGO) and functionalized with cyanuric chloride (SPGO-CC) to serve as solid support for the covalent immobilization of enzymes. Xylanase was attached to the functionalized nanocomposite with a yield of 215 mg protein per gram SPGO-CC. The kinetic constants of the immobilized (of the free soluble) xylanase are K-m = 4.9 (4.1) mg/mL, v(max), = 1.6 (1.7) mu mol min(-1) mL(-1), and k(cat) = 82 (91) min(-1), indicating a minimal impairment of catalytic activity by covalent coupling. The immobilized xylanase has shallow pH and temperature optima of 6.5 and 60 degrees C. It retains 70% of the original activity after 10 cycles of 15 min incubation with substrate (polymeric xylan) at 60 degrees C. It retains 80% of the original catalytic activity after 3.5 months storage at 4 degrees C, whereas the free, soluble enzyme retains only 50%. (C) 2015 Elsevier B.V. All rights reserved.
机译:固定化酶被用作生物催化剂,用于诊断中的分析目的以及大规模工业过程中的制备目的。固定化可以延长半衰期,提高稳定性,并增加酶的催化活性。它有助于从反应产物中分离和回收催化剂,并允许生物催化剂的多次使用。用超顺磁性氧化铁纳米颗粒(SPGO)装饰氧化石墨烯纳米片,并用氰尿酰氯(SPGO-CC)进行功能化,以作为酶的共价固定化的固体载体。木聚糖酶以每克SPGO-CC 215 mg蛋白质的产量附着在功能化的纳米复合材料上。固定化(游离可溶性)木聚糖酶的动力学常数为Km = 4.9(4.1)mg / mL,v(max),= 1.6(1.7)mu mol min(-1)mL(-1)和k( cat)= 82(91)min(-1),表明通过共价偶联对催化活性的损害最小。固定的木聚糖酶的pH值最浅,最适温度为6.5和60摄氏度。在60摄氏度下与底物(聚合木聚糖)一起孵育15分钟10次后,它保留了70%的原始活性。它保留了80%的原始催化活性。在4摄氏度下储存3.5个月后,其活性得以保持,而游离的可溶性酶仅保留50%。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号