Influence of the operating conditions in the acetone pulping of wheat straw on the properties of the resulting paper sheets

机译:小麦秸秆丙酮制浆中的操作条件对所得纸张性能的影响

获取原文
获取原文并翻译 | 示例

摘要

A central composite factor design was used to examine the influence of independent variables in the acetone pulping of wheat straw (processing temperature, time, and acetone: concentration) on the yield of the resulting pulp, and on various physical properties of paper sheets (breaking length, stretch, burst index. tear index and brightness) obtained from it. Equations that related each dependent variable to the different independent variables were obtained, and these reproduced the experimental results for the yield, breaking. stretch, burst index and brightness obtained at temperatures, times, and acetone concentrations over the ranges 140 180 degreesC. 60-120 min and 40-80% respectively, with errors less than 20%. Obtaining the optimum breaking length, stretch, burst index and tear index for the paper sheets (3456 m, 1.42%, 1.36 kN/g and 3.86 mNm(2)/g, respectively) entails using a high temperature: the processing time and acetone concentration only influence stretch, optimization of which requires using a short time and a low concentration. The optimum brightness (30.44%) is achieved with a low temperature. a short time and a medium acetone concentration. In order to minimize losses of solvent during its recovery and recycling while ensuring acceptable levels of the properties of the paper sheets, a high temperature, a low acetone concentration and a short time can be used; the brightness level thus obtained is only 10% lower than the optimum value. (C) 2001 Elsevier Science Ltd. All rights reserved. [References: 33]
机译:中央复合因子设计用于检查麦草丙酮制浆中的自变量(加工温度,时间和丙酮:浓度)对所得纸浆产量以及纸张各种物理性能(破碎)的影响。长度,拉伸,破裂指数,撕裂指数和亮度)。获得了将每个因变量与不同自变量相关联的方程,这些方程再现了屈服,断裂的实验结果。在140 180摄氏度的温度,时间和丙酮浓度下获得的拉伸,破裂指数和亮度。 60-120分钟和40-80%,误差小于20%。要获得最佳的纸张断裂长度,拉伸强度,破裂指数和撕裂指数(分别为3456 m,1.42%,1.36 kN / g和3.86 mNm(2)/ g),需要使用高温:处理时间和丙酮浓度只影响拉伸,而拉伸的优化则需要使用短时间和低浓度。在低温下可获得最佳亮度(30.44%)。时间短,丙酮浓度适中。为了最大程度地减少溶剂在其回收和再循环期间的损失,同时确保可接受的纸张性能水平,可以使用高温,低丙酮浓度和短时间。这样获得的亮度水平仅比最佳值低10%。 (C)2001 Elsevier ScienceLtd。保留所有权利。 [参考:33]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号