Calcined basic nickel carbonate (BNC) concentrate was smelted in a pilot-scale DC arc furnace to produce a nickel metal. The furnace was continuously operated for 12 days (24 hour/day), during which twelve different smelting conditions were investigated, with the major variables being reductant type and feed rate, flux composition and addition, and BNC feed rate.The 200 kW DC arc furnace was operated at power levels between 110 and 165 kW and at a total feed rate of 78 to 96 kg/h, resulting in an average slag and metal tapping temperature of about 1650°c. A total of 7.2t of BNC were smelted, producing about 5.441 of nickel metal and 2.94 t of slag. Nickel recoveries of 96.4% and higher were achieved, and the slag nickel content was as low as 0.1%. The major impurities in the metal were iron (mostly from oxygen lancing) and carbon. The calculated feed carry-over was less than 0.85% and the graphite electrode consumption was between 2.8-3.3 kg/MWh.
机译:将煅烧的碱性碳酸镍(BNC)精矿在中试规模的直流电弧炉中冶炼,以生产镍金属。该炉连续运行12天(24小时/天),在此期间研究了十二种不同的熔炼条件,主要变量为还原剂类型和进料速度,助熔剂组成和添加量以及BNC进料速度.200 kW直流电弧该炉的功率水平在110至165 kW之间,总进料速度为78至96 kg / h,平均炉渣和金属出铁温度约为1650°c。总共冶炼了7.2吨BNC,生产了约5.441镍金属和2.94吨炉渣。镍回收率达到96.4%或更高,炉渣镍含量低至0.1%。金属中的主要杂质是铁(主要来自氧气喷枪)和碳。计算的进料残留量小于0.85%,石墨电极消耗量在2.8-3.3 kg / MWh之间。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号