Feasible recycling of industrial waste coal fly ash for preparation of anorthite-cordierite based porous ceramic membrane supports with addition of dolomite

机译:可行的工业废粉煤灰回收再利用以添加白云石来制备钙锰矿-堇青石基多孔陶瓷膜载体

获取原文
获取原文并翻译 | 示例
       

摘要

Recycling of industrial solid state waste is always the priority solution in the prospect of waste management. This work demonstrated a new method converting coal fly ash (CFA) industrial waste to anorthite-cordierite-based porous ceramic membrane supports (ACCMS), through high-temperature sintering with additions of dolomite mineral. Characterization of as-prepared ACCMS included phase composition, microstructure, pore structure, N-2 and water permeability, and mechanical properties. From dilatometric measurements, the densification temperature of a sample with 28.43 wt.% dolomite addition was extended to 1100 degrees C compared to 1060 degrees C for that of a sample without any dolomite. For samples sintered at 1150 degrees C, their open porosity increased from 25.2 +/- 0.5% to 46.5 +/- 0.2% when dolomite addition increased from 0 to 28.43 wt.%. It is suggested that this level of dolomite addition significantly inhibited the sintering behavior of CFA. (C) 2015 Elsevier Ltd. All rights reserved.
机译:工业固体废物的回收一直是废物管理前景中的优先解决方案。这项工作证明了一种新方法,即通过高温烧结和添加白云石矿物,将粉煤灰(CFA)工业废料转化为基于钙长石-堇青石的多孔陶瓷膜载体(ACCMS)。所制备的ACCMS的表征包括相组成,微观结构,孔结构,N-2和水渗透性以及机械性能。通过膨胀测量,将添加28.43重量%白云石的样品的致密化温度扩展至1100℃,相比之下,不添加白云石的样品的致密化温度为1060℃。对于在1150摄氏度下烧结的样品,当白云石的添加量从0增加到28.43 wt。%时,其开孔率从25.2 +/- 0.5%增加到46.5 +/- 0.2%。这表明白云石的添加水平显着抑制了CFA的烧结行为。 (C)2015 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号