The present paper deals with the mineralogical and flotation characteristics of two lead-zinc ore samples (S1 and S2) from Ganesh-Himal region of Nepal. The two samples assayed 2.47% & 3.53% Pb and 13.6 & 13.45% Zn respectively. The ore was predominantly made up of spahlerite and pyrite in association with subordinate amounts of galena, minor amounts of pyrrhotite and chalcopyrite. Dolomite was the main gangue. The modal analysis showed the probability of fair liberation of sulphides from gangues around 210 micron but the locking of galena with sphalerite and other sulphides continued to finer sizes. However, sample S2 showed the presence high content of mineral fines and oxidised mineral phases. Detailed flotation studies carried out on the samples under varying process conditions resulted in reasonably high recovery of lead and zinc bearing minerals for sulphidic sample (SI) but recovery from oxidised sample (S2) was not satisfactory. Use of new alkyl quinoline based chelating type collector found helpful in improving flotation results.
机译:本文研究了尼泊尔加涅什-希马尔地区的两个铅锌矿石样品(S1和S2)的矿物学和浮选特性。这两个样品分别测定了2.47%和3.53%的Pb和13.6和13.45%的Zn。矿石主要由闪锌矿和黄铁矿以及少量方铅矿,少量黄铁矿和黄铜矿组成。白云石是主要的脉石。模态分析表明,大约210微米左右的脉石中的硫化物有可能从中释放出来,但方铅矿与闪锌矿和其他硫化物的锁定继续达到更细的尺寸。然而,样品S2显示出高含量的矿物细粉和氧化的矿物相。在不同的工艺条件下对样品进行的详细浮选研究导致对硫化物样品(SI)的含铅和锌矿物的回收率相当高,但从氧化样品(S2)的回收率并不令人满意。发现使用新的基于烷基喹啉的螯合型捕收剂有助于改善浮选结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号