Hollow microspheres of nickel hydroxide and nickel oxide were prepared with as-synthesized PS/Ni(OH)j composite particles by sacrificing core method, respectively. The composite particles were synthesized by deposition of the Ni(OH)2 nanoflakelets formed by the hydrolysis of nickel nitrate onto the surfaces of polystyrene (PS) particles. The effects of different concentrations of nickel salt and urea on the deposition of the nanoflakelets of nickel hydroxide were studied. It was found that the uniform nanoflakelets were deposited on the polystyrene particles under the conditions of the 4X10"3 M nickel salt and 0.667M urea. Compared with the directly calcinating of composite particles, Integral hollow microspheres of nickel hydroxide were attained by removal of cores of polystyrene in composite particles with toluene and NiO hollow microspheres by calcinating of these Ni(OH)2 hollow spheres in oven at 600℃for 2h.
机译:采用牺牲核法分别制备了PS / Ni(OH)j复合粒子,制备了氢氧化镍和氧化镍空心微球。通过将由硝酸镍水解形成的Ni(OH)2纳米片沉积到聚苯乙烯(PS)粒子的表面上来合成复合粒子。研究了不同浓度的镍盐和尿素对氢氧化镍纳米片沉积的影响。结果表明,在4×10“ 3 M的镍盐和0.667M的尿素的条件下,均匀的纳米片被沉积在聚苯乙烯颗粒上。与直接煅烧复合颗粒相比,通过去除核获得了完整的氢氧化镍空心微球。甲苯和NiO空心微球复合颗粒中的聚苯乙烯的合成,方法是将这些Ni(OH)2空心球在烘箱中于600℃下煅烧2h。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号