Properties of rubber lining after sixteen years operation in different places of FGD plant

机译:在烟气脱硫工厂不同地方运行16年后的橡胶衬里性能

获取原文
获取原文并翻译 | 示例

摘要

After over 16 years of service at the inner walls of a steel absorber and outlet channel in wet FGD system, the rubber lining was subjected to examinations. A series of impedance spectra for the pre-vulcanized soft rubber lining based on chlorobutyl rubber (CIIR) were recorded. Rubber lining samples taken from the absorber bottom, which had been in contact with the washer sump solution, exhibited properties similar to those of new rubber lining samples not exposed to the corrosive environment. Rubber lining samples taken from the absorber upper part and from the outlet channel showed significant damage, and so deterioration in their protective properties, in comparison with the new lining. Also the results of tensile strength and hardness tests carried out on rubber samples taken from various parts of the absorber and the outlet channel are presented.
机译:在湿法烟气脱硫系统中的钢制吸收器内壁和出口通道上服务超过16年后,对橡胶衬里进行了检查。记录了基于氯丁基橡胶(CIIR)的预硫化软橡胶衬里的一系列阻抗谱。从吸收塔底部取下的橡胶衬里样品已经与清洗液池溶液接触,其性能类似于未暴露于腐蚀性环境的新橡胶衬里样品。与新衬里相比,从吸收器上部和出口通道中抽取的橡胶衬里样品显示出明显的损坏,因此其防护性能下降。还显示了对从吸收器和出口通道的各个部分采集的橡胶样品进行的拉伸强度和硬度测试的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号