Mixed interior wood panel tannin adhesive formulations were developed in which lignin was in considerable proportion, 50%, of the wood panel binder, and in which no 'fortification' with synthetic resins, such as isocyanates or phenol-formaldehyde resins as used in the past, was necessary to obtain results satisfying relevant standards. A low molecular mass lignin obtained industrially by formic acid/acetic acid pulping of wheat straw was used. Environment-friendly, non-toxic polymeric materials of natural origin constitute up to 94% of the total panel binder. The wood panel itself is constituted of 99.5% natural materials, the balance 0.5% being composed of glyoxal, a non-toxic and non-volatile aldehyde, and of hexamine already accepted as a non-formaldehyde-yielding compound when in presence of very reactive chemical species such as a flavonoid tannin. Particleboards and two types of plywoods were shown to pass the relevant interior standards with such adhesive formulations. Moreover, the much cheaper non-purified organosolv lignin showed the same level of results as the more expensive purified type.
机译:开发了混合的室内木板单宁粘合剂配方,其中木质素占木板粘合剂的相当比例(50%),并且过去不使用合成树脂(例如异氰酸酯或酚醛树脂)进行“强化”是获得符合相关标准的结果所必需的。使用通过麦秆的甲酸/乙酸制浆在工业上获得的低分子量木质素。天然无污染的环保无毒聚合物材料占面板粘合剂总量的94%。木板本身由99.5%的天然材料组成,其余0.5%由乙二醛,一种无毒且不挥发的醛,以及当存在非常活泼的反应性时已被接受为非甲醛生成化合物的六胺组成化学物质,例如类黄酮单宁。刨花板和两种胶合板被证明通过了此类胶粘剂配方的相关内部标准。此外,便宜得多的未纯化有机溶剂木质素显示出与更昂贵的纯化类型相同的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号